Factory Direct Sales Constantan CuNi44 Copper-Nickel Alloy Wire

Short Description:

Constantan Wire for Sampling Resistor is a copper-nickel alloy usually consisting of 55% Copper and 45% Nickel. Its main feature is its resistance which is constant over a wide range of temperatures. It is also called Alloy 294, Nico, MWS-294, Cupron, Copel, Alloy 45, Neutrology, Advance, CuNi 44, CuNi 44, CN49.Other grades of copper nickel alloy are as follows: CN5, CuNi2 A60, Alloy 60, 60 Alloy, MWS-60, Lohm, HAI-60, CuNi 6, Alloy 260, Nickel Alloy 60, CN10 CuNi10, CN15 A30, Alloy 30, CuNi23, 30 Alloy, MWS-30, HAI-30, Alloy 230, Nickel Alloy 30, CN 30 CuNi1, CuNi15, CuNi30


Product Detail

FAQ

Product Tags

Factory Direct Sales Constantan CuNi44 Copper-Nickel Alloy Wire

Constantan Wire for Sampling Resistor is a copper-nickel alloy usually consisting of 55% Copper and 45% Nickel. Its main feature is its resistance which is constant over a wide range of temperatures. It is also called Alloy 294, Nico, MWS-294, Cupron, Copel, Alloy 45, Neutrology, Advance, CuNi 44, CuNi 44, CN49.
Other grades of copper nickel alloy are as follows:
CN5, CuNi2
A60, Alloy 60, 60 Alloy, MWS-60, Lohm, HAI-60, CuNi 6, Alloy 260, Nickel Alloy 60, CN10
CuNi10, CN15
A30, Alloy 30, CuNi23, 30 Alloy, MWS-30, HAI-30, Alloy 230, Nickel Alloy 30, CN 30
CuNi1, CuNi15, CuNi30

If thee is any question or requirement, pls be free to contact with us.

Properties/Grade CuNi1 CuNi2 CuNi6 CuNi8 CuNi10
Max Continuous Service Temperature(º C) 200 200 200 250 250
Resisivity at 20º C  (Ω mm2/m) 0.03 0.05 0.1 0.12 0.15
Density(g/cm 3 ) 8.9 8.9 8.9 8.9 8.9
Thermal Conductivity(α × 10 -6 /º C) < 100 < 120 < 60 < 57 < 50
Tensile Strength(Mpa) 210 220 250 270 290
EMF vs Cu(μ V/º C)(0~1000º C) -8 -12 -12 -22 -25
Approximate Melting Point( º C) 1085 1090 1095 1097 1100
             
Properties/Grade CuNi14 CuNi19 CuNi23 CuNi30 CuNi44
Max Continuous Service Temperature(º C) 300 300 300 350 400
Resisivity at 20º C  (Ω mm2/m) 0.2 0.25 0.3 0.35 0.5
Density(g/cm 3 ) 8.9 8.9 8.9 8.9 8.9
Thermal Conductivity(α × 10 -6 /º C) < 30 < 25 < 16 < 10 < -6
Tensile Strength(Mpa) 310 340 350 400 420
EMF vs Cu(μ V/º C)(0~1000º C) -28 -32 -34 -37 -43
Approximate Melting Point( º C) 1115 1135 1150 1170 1200