FeCrAl alloys are characterized by excellent oxidation resistance and very good form stability resulting in long element life.

They are typically used in electrical heating elements in industrial furnaces and home appliances.

 

Fe-Cr-Al alloy with high resistivity and serviceability temperature than that for NiCr alloy and also has lower price.

 

Applications

Iron-chrome-aluminium electric resistor strip is widely used for making electric heating elements in home appliances and industrial furnaces. Typical applications are flat irons, ironing machines, water heaters, plastic moulding dies, soldering irons, metal sheathed tubular elements and cartridge elements
Application area

Our products are widely used in heat treatment equipment, auto parts, iron and steel manufacturing,

aluminum industry, metallurgical equipment, petrochemical equipment, glass machinery, ceramic machinery,

food machinery, pharmaceutical machinery, and power engineering industry.
Chemical Content, %

Alloy material Chemical composition %
C P S Mn Si Cr Ni Al Fe others
max(≤)
1Cr13Al4 0.12 0.025 0.025 0.7 ≤1.00 12.5-15.0 - 3.5-4.5 Rest -
0Cr15Al5 0.12 0.025 0.025 0.7 ≤1.00 14.5-15.5 - 4.5-5.3 Rest -
0Cr25Al5 0.06 0.025 0.025 0.7 ≤0.60 23.0-26.0 ≤0.60 4.5-6.5 Rest -
0Cr23Al5 0.06 0.025 0.025 0.7 ≤0.60 20.5-23.5 ≤0.60 4.2-5.3 Rest -
0Cr21Al6 0.06 0.025 0.025 0.7 ≤1.00 19.0-22.0 ≤0.60 5.0-7.0 Rest -
0Cr19Al3 0.06 0.025 0.025 0.7 ≤1.00 18.0-21.0 ≤0.60 3.0-4.2 Rest -
0Cr21Al6Nb 0.05 0.025 0.025 0.7 ≤0.60 21.0-23.0 ≤0.60 5.0-7.0 Rest Nb add0.5
0Cr27Al7Mo2 0.05 0.025 0.025 0.2 ≤0.40 26.5-27.8 ≤0.60 6.0-7.0 Rest

Main technical characteristics of FeCrAl Alloy:

Brand

Property

1Cr13Al4 1Cr21Al4 0Cr21Al6 0Cr23Al5 0Cr25Al5 0Cr21Al6Nb 0Cr27Al7Mo2
Major chemical component% Cr 12.0-12.5 17.0-21.0 19.0-22.0 20.5-23.5 23.0-26.0 21.0-23.0 26.5-27.8
Al 4.0-6.0 2.0-4.0 5.0-7.0 4.2-5.3 4.5-6.5 5.0-7.0 6.0-7.0
Fe Balance Balance Balance Balance Balance Balance Balance
Re Appropriate Appropriate Appropriate Appropriate Appropriate Appropriate Appropriate
Addition Nb:0.5 Addition

Mo:1.8-2.2

Component max. use temperature 950 1100 1250 1250 1250 1350 1400
Melting Point 1450 1500 1500 1500 1500 1510 1510
Density g/cm3 7.40 7.35 7.16 7.25 7.10 7.10 7.10
Resistivity μΩ·m,20 1.25±0.08 1.23±0.06 1.42±0.07 1.35±0.06 1.45±0.07 1.45±0.07 1.53±0.07
Tensile Strength Mpa 588-735 637-784 637-784 637-784 637-784 637-784 684-784
Extension rate% 16 12 12 12 12 10
Repeated bending frequency 5 5 5 5 5
Fast lift h/ - 80/1300 80/1300 50/1350
Specific Heat J/g. 0.490 0.490 0.520 0.460 0.494 0.494 0.494
Heat Conduction Coefficient KJ/M.h 52.7 46.9 63.2 60.1 46.1 46.1 45.2
Linear expansion coefficient aX10-6/

(20-1000)

15.4 13.5 14.7 15.0 16.0 16.0 16.0
Hardness HB 200-260 200-260 200-260 200-260 200-260 200-260 200-260
Microstructure Ferritic Ferritic Ferritic Ferritic Ferritic Ferritic Ferritic
Magnetic Magnetic Magnetic Magnetic Magnetic Magnetic Magnetic Magnetic