Designation |
1J85
|
Correspoding Standard
|
GB /T 32286.1-2015
|
Label
|
High Magnetic Permeability Nickel-Iron Alloy
|
Description
|
Recommended Heat Treatment Process:
* Heating Temperature: 1100-1200°C * Soaking Time: 3-6 hours * Cooling Process: Cool from 100-200°C/h to 500-600°C, then cool at no less than 400°C/h to below 300°C before removal. Basic Physical Parameters: |
Density
|
8.75 g/cm3
|
Chemical Components
|
|||||||||
Components
|
C
|
Si
|
Mn
|
P
|
S
|
Ni
|
Cu
|
Mo
|
More
|
Max
|
0.03
|
0.3
|
0.6
|
0.02
|
0.02
|
81
|
0.2
|
5.2
|
Fe Balance
|
Min
|
-
|
0.15
|
0.3
|
-
|
-
|
79
|
-
|
4.8
|