Welcome to our websites!

High Temperature Coefficient MWS-30 for Temperature Sensitive Resistors

Short Description:

Alloy exhibits low resistivity and high temperature coefficient of resistance. Typical applications include voltage regulators, timing devices, temperature sensitive resistors, temperature compensating devices, motor control, heating wires and cables, precision and vitreous resistors, potentiometers, and low temperature heating applications.


  • Grade: MWS-30
  • Size: 0.1mm~1mm
  • Usages: Motor Control
  • Max operating temp(uΩ/m at 20°C): 0.3
  • Density(g/cm³): 8.9
  • Elongation(%): ≥25
  • Product Detail

    FAQ

    Product Tags

         Copper Nickel (CuNi) alloys are medium to low resistance materials typically used in applications with maximum operating temperatures up to 400°C (750°F).

         With low temperature coefficients of electrical resistance, resistance, and thus performance, is consistent regardless of temperature. Copper Nickel alloys mechanically boast good ductility, are easily soldered and welded, as well as have outstanding corrosion resistance. These alloys are typically used in high current applications requiring a high level of precision.

         Alloy exhibits low resistivity and high temperature coefficient of resistance. Typical applications include voltage regulators, timing devices, temperature sensitive resistors, temperature compensating devices, motor control, heating wires and cables, precision and vitreous resistors, potentiometers, and low temperature heating applications.

    Grade CuNi44 CuNi23 CuNi10 CuNi6 CuNi2 CuNi1 CuNi8 CuNi14 CuNi19 CuNi30 CuNi34 CuMn3
    Cuprothal 49 30 15 10 5
    Isabellehutte ISOTAN Alloy 180 Alloy 90 Alloy 60 Alloy 30 ISA 13
    Nominal composition% Ni 44 23 10 6 2 1 8 14 19 30 34
    Cu Bal Bal Bal. Bal. Bal. Bal. Bal. Bal. Bal Bal Bal Bal
    Mn 1 0.5 0.3 0.5 0.5 1.0 1.0 3.0
    Max operating temp(uΩ/m at 20°C) 0.49 0.3 0.15 0.10 0.05 0.03 0.12 0.20 0.25 0.35 0.4 0.12
    Resisivity (Ω/cmf at 68°F) 295 180 90 60 30 15 72 120 150 210 240 72
    Max operating temp(°C) 400 300 250 200 200 200 250 300 300 350 350 200
    Density(g/cm³) 8.9 8.9 8.9 8.9 8.9 8.9 8.9 8.9 8.9 8.9 8.9 8.9
    TCR(×10-6/°C) <-6 <16 <50 <60 <120 <100 <57 <30 <25 <10 <0 <38
    Tensile Strength(Mpa ) ≥420 ≥350 ≥290 ≥250 ≥220 ≥210 ≥270 ≥310 ≥340 ≥400 ≥400 ≥290
    Elongation(%) ≥25 ≥25 ≥25 ≥25 ≥25 ≥25 ≥25 ≥25 ≥25 ≥25 ≥25 ≥25
    EMF vs Cu  uV/°C(0~100°C) -43 -34 -25 -12 -12 -8 22 -28 -32 -37 -39 -
    Melting Point (°C) 1280 1150 1100 1095 1090 1085 1097 1115 1135 1170 1180 1050
    Magnetic Property non non non non non non non non non non non non