FeCrAl Alloy Strip 1Cr13Al4 , 1Cr13Al4 Heating Resistance Strip for Furnace Elements

Short Description:

FeCrAl alloy strip 1Cr13Al4, high electrical resistivity and excellent oxidation resistance up to 1100°C. Low density, long service life, ideal for industrial furnace heating elements, electric heaters, and high-temperature kilns. Thickness from 0.5mm to 5.0mm, width up to 400mm. Stable quality, ISO certified. Suitable for both continuous and intermittent operation.


  • Certificate: ISO 9001
  • Size: Customized
  • Alloy Grade: 1Cr13Al4 (FeCrAl)
  • Max Operating Temp: 1100°C
  • Resistivity: ~1.25 μΩ·m @20°C
  • Density: 7.4 g/cm³
  • Thickness: 0.5mm – 5.0mm (custom)
  • Width: 5mm – 400mm
  • Applications: Furnace elements, electric heaters
  • Product Detail

    FAQ

    Product Tags

    Product Description

    FeCrAl Allloy Strip (1Cr13Al14/CrAl14/FeCrAl134)
    Nominal Analysis

    14.00 Cr, 4.00 Al, Bal. Fe

    Max contineous working temperature: 950º C.

    Melting Temperature: 1450º C

    Electrical Resistivity: 1.25 ohm mm2/m

    Has been used extensively as heating elements in industrial furnaces and electrical kilns.

    Has less hot strength than Tophet alloys but much higher melting point.

    Shanghai TANKII ALLOY MATERIAL CO., LTD.

    ALCHROME ALLOY PRODUCER IN CHINA

    Chemical Composition and Main Property of Fe-Cr-Al Resistance Alloy
    Properties \ Grade 1Cr13Al4 0Cr25Al5 0Cr21Al6 0Cr23Al5 0Cr21Al4 0Cr21Al6Nb 0Cr27Al7Mo2
    Main Chemical Composition
    (%)
    Cr 12.0-15.0 23.0-26.0 19.0-22.0 22.5-24.5 18.0-21.0 21.0-23.0 26.5-27.8
    Al 4.0-6.0 4.5-6.5 5.0-7.0 4.2-5.0 3.0-4.2 5.0-7.0 6.0-7.0
    Re opportune opportune opportune opportune opportune opportune opportune
    Fe Bal. Bal. Bal. Bal. Bal. Bal. Bal.
    Nb0.5 Mo1.8-2.2
    Max Continuous Service Temperature(oC) 950 1250 1250 1250 1100 1350 1400
    Resisivity 20oC (Ωmm2/m) 1.25
    ±0.08
    1.42
    ±0.06
    1.42
    ±0.07
    1.35
    ±0.07
    1.23
    ±0.07
    1.45
    ±0.07
    1.53
    ±0.07
    Density(g/cm3) 7.4 7.1 7.16 7.25 7.35 7.1 7.1
    Thermal Conductivity 52.7 46.1 63.2 60.2 46.9 46.1 45.2
    (KJ/m@h@oC)
    Coefficient of Thermal Expansion(α×10-6/oC) 15.4 16 14.7 15 13.5 16 16
    Approximate Melting Point( oC) 1450 1500 1500 1500 1500 1510 1520
    Tensile Strength(N/mm2) 580-680 630-780 630-780 630-780 600-700 650-800 680-830
    Elongation(%) >16 >12 >12 >12 >12 >12 >10
    Section Variation 65-75 60-75 65-75 65-75 65-75 65-75 65-75
    Shrink Rate (%)
    Repeatedly Bend Frequency(F/R) >5 >5 >5 >5 >5 >5 >5
    Hardness (H.B.) 200-260 200-260 200-260 200-260 200-260 200-260 200-260
    Continuous Service Time no ≥80/1300 ≥80/1300 ≥80/1300 ≥80/1250 ≥50/1350 ≥50/1350
    Micrographic Structure Ferrite Ferrite Ferrite Ferrite Ferrite Ferrite Ferrite
    Magnetic Property Magnetic Magnetic Magnetic Magnetic Magnetic Magnetic Magnetic

    FeCrAl Alloy Strip 1Cr13Al4 , 1Cr13Al4 Heating Resistance Strip for Furnace Elements

    FeCrAl Alloy Strip 1Cr13Al4 , 1Cr13Al4 Heating Resistance Strip for Furnace Elements
    FeCrAl Alloy Strip 1Cr13Al4 , 1Cr13Al4 Heating Resistance Strip for Furnace Elements
    FeCrAl Alloy Strip 1Cr13Al4 , 1Cr13Al4 Heating Resistance Strip for Furnace Elements
    FeCrAl Alloy Strip 1Cr13Al4 , 1Cr13Al4 Heating Resistance Strip for Furnace Elements

     


  • Previous:
  • Next:

  • Write your message here and send it to us